  Heilongjiang putty powder wholesaleWhat if the manufacturer tells you how to depowder the surface of putty powder
  Cause:
  1, construction reasons: due to the paint master after the finishing construction with a scraper for many times to dry the wall caused by the surface of the fine peeling phenomenon, such as dry will form the symptoms of depowder。
  2, human reasons: due to the latter construction putty is not dry, encounter foreign dust attached to the wall caused by the wall illusion depowder。

  3, production reasons: due to the production staff careless proportion of raw material formula misplaced, or due to machine equipment failure, resulting in formula instability caused by depowder。

Heilongjiang putty powder批发" alt="Heilongjiang putty powder wholesale" />



  Heilongjiang putty powderSurface depowder treatment method:
  1, the construction master should pay attention to the surface humidity of the putty when the construction is not painted, it will cause peeling and powder when it is too dry, and the knife marks can be smoothed when the finishing is done, and it should not be dry scraped many times。
  2, such as dust attached to the wall caused by the illusion of dedusting, should be completed after the decoration with feather duster dust, or clean with water and clean cloth can be wiped clean。
  3, such as the emergence of fast dry depowder, should wait for the company's technical personnel to the scene to identify whether it is due to the cause of product formulation。
  Note: If it is the product formula problem, the symptoms should be: bad batch scraping, fast drying, dry after the putty layer is relatively loose, easy to powder, easy to crack and other phenomena。